MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Blue River Coatings Wood Primer
Categories: Polymer; Adhesive; Thermoset

Material Notes: BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating. BLUE RIVER COATINGS WOOD PRIMER has been tested and approved by the Window Door Manufacturer Association (WDMA).

Enviromental Advantages:BLUE RIVER COATINGS WOOD PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent adhesion to wood preservatives
  • Solvent resistant
  • Can be applied in a wide variety of temperature and humidity conditions without the use of retarders
  • Distilled water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Can be oven baked
  • Wide range of colors
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Will not support combustion
  • Excellent water repellency
  • Household cleaner resistant
  • Uses

  • Wood windows and doors
  • Pre-Finished siding
  • Salt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654-Passed 500 hours.

    Primer has been tested and approved for use by Sealrite Windows, Inc., including an actual 18-month exterior weather test at the Sealrite plant in Nebraska. Also approved by Windsor Windows in Iowa and North Carolina.

    Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity >= 1.00 g/cc
    Density 10.36 lb/gal
    Solids Content 40.62 %by volume
     43.2 %by weight
    Volatile Organic Compounds (VOC) Content 240 g/l
    pH 7.0 - 8.5
     
    Mechanical PropertiesOriginal ValueComments
    Impact Test 80.0 in-lb
     
    Thermal PropertiesOriginal ValueComments
    Boiling Point 169 °C
    Flash Point 150 °F
     
    Processing PropertiesOriginal ValueComments
    Cure Time 0.100 hour
    @Temperature 140 °C
    Dry to stack, at 50% humidity
     0.167 hour
    @Temperature 75.0 °C
    Dust Free, at 50% humidity
     0.330 hour
    @Temperature 75.0 °C
    Recoat, at 50% humidity
     0.500 hour
    @Temperature 75.0 °C
    Dry to handle, at 50% humidity and 75°C
    Shelf Life 12.0 Month
     
    Descriptive Properties
    AdhesionExcellent; preservative treated wood.
    Evaporation rateSlower than ether
    Theoretical Coverage652 ft2 at 1 mil
    Vapor DensityHeavier than air
    Water Submersion<1% water gain when submerged for 24 hours

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Inovyn 266SC Polyvinyl Chloride Pastes - filler Polymers
    BASF Heligoen® Blue L 7080 Color Additive
    A. Schulman POLYBLAK™ 2723Pm Premium Black Color Concentrate, 25% Carbon Black Based In HDPE
    Universal Wire Works ER317L Stainless Steel Bare Wire
    Allnex UCECOAT® 2501 Waterborne UV Resin

    WBLUER04 / 74603

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.