MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Devcon® Aluminum Liquid (F-2)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Aluminum-filled, pourable epoxy for making molds, patterns, and holding fixtures that can be machined, drilled, or tapped. Uses: Mold-making, patterns, holding fixtures, leveling equipment. Features: Machinable to metallic finish, Low viscosity, self-leveling liquid, Cast able, Low shrinkage.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/cc
Solids Content 100 %100 %
Viscosity 15000 - 25000 cP15000 - 25000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Modulus of Elasticity 5.17 GPa750 ksi
Flexural Strength 49.5 MPa7180 psiASTM D790
Compressive Strength 67.7 MPa9820 psiASTM D695
Shear Strength 18.6 MPa2700 psiASTM D1002
Adhesive Bond Strength 18.6 MPa2700 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 8.68.6ASTM D150
Dielectric Strength 3.94 kV/mm100 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Thermal Conductivity 0.661 W/m-K4.59 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 48.9 °C120 °FTemperature Resistance - Wet
 121 °C250 °FTemperature Resistance - Dry
Shrinkage 0.090 %0.090 %Linear During cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  960 min
@Temperature 24.0 °C
16.0 hour
@Temperature 75.2 °F
Functional cure
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
As Tested
Pot Life 75.0 min
@Temperature 23.9 °C
75.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methylene Chloride: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Chloride Brine: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 50%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Trisodium Phosphate: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Xylene: fair30 day immersion at 75°F. Sample cured 7 days at RT
ColorAluminum
Coverage70 in²/lbCured. @ 1/4"
Mix Ratio by volume5:1
Mix Ratio by weight9:1
Recoat Time2 to 4 hrs
Specific Volume (in.³/lb)17.5Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9200 / 239710

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.