MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include:
  • Excellent electrical properties
  • High thermal stability
  • Long term temperature rating up to 200°C
  • Outstanding chemical resistance
  • Wide processing window

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Melt Index of Compound 7.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaASTM D638
Elongation at Break 350 %ASTM D638
Flexural Modulus 0.580 GPaASTM D790
Izod Impact, Notched NB
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant <= 2.15
@Frequency 1000 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 102 kV/mm4.5 mil film; ASTM D149
Dissipation Factor <= 0.00030
@Frequency 1000 Hz
ASTM D150
 <= 0.00070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CASTM D4591
Brittleness Temperature <= -70.0 °CASTM D746
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules
3M Dyneon™ FEP 6307 R2RZ Fluorinated Ethylene Propylene Fluorothermoplastic Granules
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules
Daikin NEOFLON® NP-21 FEP Pellets
Daikin NEOFLON® AP-231SH PFA

PDYNE003 / 34811

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.