MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Kendall® MERCON® V ATF
Categories: Fluid; Lubricant

Material Notes: Kendall® MERCON®V ATF is a premium quality, part-synthetic transmission fluid approved for use in passenger car and light truck automatic transmissions that require a Ford MERCON®V fluid. It is back serviceable for use in 2006 and earlier model-year Ford vehicles where the OEM previously specified MERCON® fluid, and also may be used in most 2005 and earlier model-year GM automatic transmissions. MERCON®V ATF is formulated to provide improved antiwear and anti-shudder performance compared with earlier-generation fluids, as well as better low-temperature properties for easier shifting in cold weather. It is highly shear stable and has excellent oxidation resistance for long fluid life. The part-synthetic formulation provides enhanced performance benefits compared with conventional, all-mineral transmission fluids.

Applications:

  • Ford automatic transmissions where MERCON®V or an earlier-generation MERCON® fluid (obsolete) is specified
  • GM automatic transmissions in 2005 and earlier vehicles, except those that require DEXRON®-VI for warranty coverage, or a Type T-IV or CVT fluid
  • Heavy-duty automatic and powershift transmissions in trucks and buses
  • Power steering systems in many newer Ford vehicles
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range
MERCON®V ATF is OEM-approved for service fill in the following applications:
  • Ford MERCON®V (License Nos. M5091001, M5091002, M5091003, M5091004, M5091005)
  • Voith DIWA transmissions
MERCON®V ATF is recommended for service fill in the following applications:
  • Allison automatic transmissions in off-highway applications where a C-4 quality fluid is specified
  • ZF Ecomat transmissions
Features/Benefits:
  • Proper frictional properties for smooth shifting and excellent anti-shudder performance
  • Excellent oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against wear
  • High shear stability
  • Protects against rust and corrosion
  • Excellent low-temperature properties for easier shifting in cold weather
  • Good seal compatibility
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.857 g/cc0.857 g/cc
Density 0.856 g/cc0.0309 lb/in³
Brookfield Viscosity 10200 cP
@Temperature -40.0 °C
10200 cP
@Temperature -40.0 °F
Viscosity Measurement 202202Index
Kinematic Viscosity at 40°C (104°F) 34 cSt34 cSt
Kinematic Viscosity at 100°C (212°F) 7.6 cSt7.6 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -45.0 °C<= -49.0 °F
Flash Point 196 °C385 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn <= 0.0010 %<= 0.0010 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON6467 / 210048

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.