Rolled and Molded Rods made from a plain weave, medium weight cotton fabric combined with a phenolic resin system. RM310 is used for mechanical applications, meeting ANSI/NEMA IM 60000-2021 Grade C, MIL-I-24768/16 FBM and ASTM D709 Type II Grade C requirements.Information provided by Norplex Micarta. |
Cotton Fiber, Phenolic, ANSI/NEMA IM 60000-2021 Grade C, MIL-I-24768/16 FBM, ASTM D709 Type II Grade C |