MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Avient Versaflex™ HC MT317 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial specifications have not been established.

Rear: 330 to 370F Center: 350 to 400F Front: 360 to 420F Screw speed: 100 to 500 RPM Drying is not required Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Versaflex™ HC MT317. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). The use of regrind is not recommended for Versaflex™ HC MT317.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.888 g/cc0.888 g/ccASTM D792
Viscosity  10000 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
10000 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 52000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
52000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.013 - 0.017 cm/cm0.013 - 0.017 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 686810 sec; ASTM D2240
Tensile Strength at Break 6.00 MPa
@Temperature 23.0 °C
870 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain  3.10 MPa
@Strain 100 %,
Temperature 23.0 °C
450 psi
@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
 4.55 MPa
@Strain 300 %,
Temperature 23.0 °C
660 psi
@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 470 %
@Temperature 23.0 °C
470 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set  17 %
@Temperature 22.0 °C,
Time 79200 sec
17 %
@Temperature 71.6 °F,
Time 22.0 hour
ASTM D395B
 58 %
@Temperature 70.0 °C,
Time 79200 sec
58 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 69 %
@Temperature 100 °C,
Time 79200 sec
69 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Die Temperature 182 - 216 °C360 - 421 °F
Melt Temperature 182 - 204 °C360 - 399 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Agency RatingsISO 10993 Part 4
 ISO 10993 Part 5
AppearanceTranslucent
FeaturesGood Color Stability
 Good Flexibility
 Kink Resistant
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesMedical/Healthcare Applications
 Tubing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Avient Versaflex™ HC MT226 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT224 Thermoplastic Elastomer (TPE)

PH0POL1258 / 145827

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.