MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dielectric Polymers NT-240APS High Temperature Laminating Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: Acrylic adhesive with moisture stable PE coated kraft (60#) liner.

Features:

  • Plasticizer migration resistant
  • High temperature shear properties
  • Neutral pH
  • Solvent resistant

Applications:

Interior automotive and kiss cut applications, mounting photos and graphic materials and bonding a variety of substrates where elevated temperatures are a critical consideration.

Information provided by Dielectric Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 102 microns4.00 milAdhesive
 102 microns4.00 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.789 kN/m4.50 pli180° peel, PET/s.s.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °FContinuous
 232 °C450 °FIntermittent
 232 °C450 °FShear Adhesive Failure (cohesive failure)
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
Abatron Water Epoxy Floor Coating System
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete

PDIEL25 / 30140

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.