MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

P & P Technology Silver/Aluminum Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exposed to atmospheric moisture.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.86 g/cc1.86 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868
Tensile Strength 1.79 MPa260 psi
Elongation at Break >= 155 %>= 155 %
Shear Strength >= 1.21 MPa>= 175 psi
Tear Strength >= 45.0 kN/m>= 257 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.010 ohm-cm0.010 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 400 °C752 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min0.250 hourSkin over
 720 - 1440 min12.0 - 24.0 hourCure for Handling
 4320 - 8640 min72.0 - 144 hourFull Cure
Tack-Free Time 90.0 min1.50 hour
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
Kotec Carbotex KV-20FD Polycarbonate, Food Grade
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy

PPPTEC030 / 133494

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.