MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Excalibar NewWate™ Barite BaSO4 Powder
Categories: Ceramic; Other Engineering Material

Material Notes: NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate™ is chemically inert to all drilling fluid additives and is applicable to all drilling fluids for purposes of increasing density.

Water Soluble Alkaline Earth Metals as Calcium <250 mg/kg.

Information provided by Excalibar Minerals LLC.

Key Words: Baryte, BaSO4, Barium Sulfate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.10 g/cc4.10 g/cc
Bulk Density 1.46 g/cc0.0527 lb/in³Loose
 2.35 g/cc0.0851 lb/in³Packed
Moisture Absorption 0.1 %0.1 %
Particle Size 6.0 µm6.0 µm< 30 wt% below (equivalent spherical diameter)
 15 µm15 µmMedian
 <= 75 µm<= 75 µm< 3.0 wt% above
 <= 80 µm<= 80 µmTop Size
Particle Mesh Size 200 Mesh200 Mesh98.0% passes
pH 88

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BACT DLC Diamond-Like Coating
A-Glass Fiber, Generic
MarkeTech Gallium Phosphide Semiconductor Wafer, n-type, Sulfur + Tellurium Doped, Czochralski-LEC Grown
Ferro CeZrO2 Grinding Media
Ferro Aluminum Oxide Grinding Media P87

CEXCAL960 / 176041

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.