MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC 350 Thermoset Polyester, Medium Impact
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.

Typical applications are small appliance end panels, control panels, bases and large appliance handles, vent trim and control panels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 - 1.95 g/cc1.85 - 1.95 g/cc
Water Absorption 0.15 - 0.25 %0.15 - 0.25 %24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 40 - 5040 - 50
Tensile Strength, Ultimate 41.4 - 48.3 MPa6000 - 7000 psi
Flexural Strength 82.7 - 110 MPa12000 - 16000 psi
Flexural Modulus 11.0 - 12.4 GPa1600 - 1800 ksi
Compressive Strength 124 - 138 MPa18000 - 20000 psi
Izod Impact, Notched 1.60 - 2.67 J/cm3.00 - 5.00 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C425 - 500 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
Overview of materials for Vinyl Ester Sheet Molding Compound
A. Schulman BMC 304 Automotive Grade Molding Compound
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 324 Automotive Grade Molding Compound

PBMC007 / 27190

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.