MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Hyosung Topilene R530 PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: Topilene® R530 is a specially designed polypropylene random copolymer that features excellent processabillity and good clarity. It is suitable for pharmaceutical, cosmetic and food contact products. Topilene® R530 complies with FDA requirements in the code of Federal Regulations in 21 CFR 177.1520 for food contact. This product passed the US Pharmacopoeia test (USP class ?) as well as the European Pharmacopoeia test (EP 3.1.6) and can be used for medical purpose. This product also obtained the Chinese Food and Drug Administration approval and it is registered in the FDA Drug Master File list.(DMFNo.21499)

Typical Applications: Intravenous bottle(ISBM)/ Cosmetic container/ Food container/ CPP film

Features: Excellent processabillity/ High transparency

Information provided by Hyosung Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Storage Temperature 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85ASTM D785
Tensile Strength, Yield 280 kg(f)/cm²ASTM D638
Flexural Modulus 9500 kg(f)/cm²ASTM D790
Izod Impact, Unnotched 5.00 kg-cm/cmASTM D256
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 - 100 °C
Dry Time 2.00 - 4.00 hourair circulated condition
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hyosung Topilene R530A PP
Hyosung Topilene R200P PP
Constellium PLAN 5754 Aluminum Rolled Plate
304 Stainless Steel

PHYOS68 / 47954

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.