System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Material Notes:
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.
7.5% glass filled
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.35
g/cc
ASTM D792
Density
1.35
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0060
-
0.010
in/in
ASTM D955
0.0060
-
0.010
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.010
-
0.014
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
78.0
MPa
5mm/min; ISO 527-2/1A
9700
psi
ASTM D638
Tensile Strength, Yield
11500
psi
ASTM D638
Elongation at Break
8.0 %
5mm/min; ISO 527-2/1A
8.5 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus
450000
psi
@Temperature 22.8 °C
ASTM D638
Flexural Strength
105
MPa
ISO 178
16000
psi
ASTM D790
Flexural Modulus
3550
MPa
ISO 178
500000
psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched (ISO)
3.80
kJ/m²
ISO 180/1A
Izod Impact, Unnotched (ISO)
23.0
kJ/m²
ISO 180/1U
Charpy Impact Unnotched
NB
ISO 179/1eU
190
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
6.00
kJ/m²
ISO 179/1eA
5.50
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+13
ohm-cm
IEC 60093
1.00e+15
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.6
@Frequency 1e+6 Hz
IEC 60250
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength
23.0
kV/mm
IEC 60243-1
470
V/mil
short term; ASTM D149
Dissipation Factor
0.0013
@Frequency 100 Hz
IEC 60250
0.020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance
130
sec
ASTM D495
Comparative Tracking Index
250
V
ASTM D3638
Thermal Properties
Original Value
Comments
CTE, linear
130
µm/m-°C
ISO 11359-2
Specific Heat Capacity
1.97
J/g-°C
Internal
Thermal Conductivity
0.131
W/m-K
Internal
Melting Point
225
°C
10°C/min; ISO 11357-1,-2,-3
437
°F
ASTM D3418
Transformation Temperature, Tg
60.0
°C
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
206
°C
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
143
°C
ISO 75-1, -2
Vicat Softening Point
185
°C
B50 (50°C/h 50N); ISO 306
Oxygen Index
22 %
ISO 4589
Processing Properties
Original Value
Comments
Processing Temperature
20.0
-
50.0
°C
65.0
-
93.0
°C
Cavity temperature
Feed Temperature
230
-
240
°C
Rear Barrel Temperature
230
-
240
°C
Middle Barrel Temperature
235
-
250
°C
Front Barrel Temperature
240
-
260
°C
Nozzle Temperature
250
-
260
°C
Zone 1
230
-
240
°C
Zone 2
235
-
250
°C
Zone 3
235
-
250
°C
Zone 4
240
-
260
°C
Die Temperature
250
-
260
°C
Melt Temperature
240
-
260
°C
260
°C
Injection molding; ISO 294
Mold Temperature
82.0
°C
Injection molding; ISO 294
150
-
200
°F
Injection Velocity
300
mm/sec
ISO 294
Drying Temperature
120
-
130
°C
Dry Time
4.00
hour
Moisture Content
0.020 %
Necessary low maximum residual
Hold Pressure
48.0
MPa
ISO 294
Back Pressure
0.000
-
50.0
psi
Hot-Working Temperature
250
-
260
°C
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Longer pre-drying times/storage
lower the temperature to 100° C until processed.
<= 60 h
Processing conditions
ISO 7792-2
Processing Notes
Fast Injection Speed
Medium Screw Speed
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Evonik Vestodur® X9400 10% Glass Reinforced PBT
Envalior Arnite® TV6 220 PBT-GF10
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced
Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced
PHCR035 / 158602
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.