SABIC NORYL GTX™ Resin GTX202 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Polyphenylene Ether/PPO
Material Notes:
NORYL GTX™ 202 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits excellent chemical resistance and excellent paintability.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.10
g/cc
0.0397
lb/in³
ISO 1183
Moisture Absorption
0.0700 %
0.0700 %
Injection Molding
1.10 %
1.10 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
3.5 %
3.5 %
ISO 62-1
Viscosity
12
cP
@Load 5.00 kg,
Temperature 280 °C
12
cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.012
-
0.016
cm/cm
0.012
-
0.016
in/in
SABIC method
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
85.0
MPa
12300
psi
H358/30; ISO 2039-1
Tensile Strength at Break
50.0
MPa
7250
psi
50 mm/min; ISO 527
Tensile Strength, Yield
55.0
MPa
7980
psi
50 mm/min; ISO 527
Elongation at Break
20 %
20 %
50 mm/min; ISO 527
Elongation at Yield
8.0 %
8.0 %
50 mm/min; ISO 527
Tensile Modulus
2.20
GPa
319
ksi
1 mm/min; ISO 527
Flexural Strength
70.0
MPa
10200
psi
yield, 2 mm/min; ISO 178
Flexural Modulus
1.90
GPa
276
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
13.0
kJ/m²
6.19
ft-lb/in²
80*10*4; ISO 180/1A
10.0
kJ/m²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched
1.30
J/cm²
6.19
ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.00
J/cm²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles
15
15
CS-17, 1 kg; SABIC method
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
90.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Thermal Conductivity
0.230
W/m-K
1.60
BTU-in/hr-ft²-°F
ISO 8302
Hot Ball Pressure Test
125
°C
257
°F
PASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
150
°C
302
°F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Vicat Softening Point
170
°C
338
°F
Rate B/120; ISO 306
170
°C
338
°F
Rate B/50; ISO 306
Processing Properties
Metric
English
Comments
Nozzle Temperature
270
-
300
°C
518
-
572
°F
Zone 2
270
-
290
°C
518
-
554
°F
Zone 3
280
-
300
°C
536
-
572
°F
Melt Temperature
280
-
310
°C
536
-
590
°F
Injection Molding
Mold Temperature
80.0
-
120
°C
176
-
248
°F
Drying Temperature
100
-
120
°C
212
-
248
°F
Injection Molding
Dry Time
2.00
-
3.00
hour
2.00
-
3.00
hour
Injection Molding
Precipitation Temperature
60.0
-
80.0
°C
140
-
176
°F
Hopper Temperature
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH82115 / 290062
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.