MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D4158 K (O/E SBS) Radial Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D4158 K is an oiled, radial copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form:
Kraton D4158 KT - supplied as a dusted porous pellet
Kraton D4158 KU - supplied as an undusted porous pellet

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D4158 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D4025
Volatiles <= 1.0 %KM 04
Viscosity 1090 - 2050 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 33 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Ash 0.25 - 0.45 %Talc; BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 16 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 41ASTM D2240
Tensile Strength 8.96 MPaTypical values on polymer compression molded at 350ºF; ASTM D412
Elongation at Break 1110 %Typical values on polymer compression molded at 350ºF; ASTM D412
300% Modulus 0.00158 GPa
@Strain 300 %
compression molded at 350ºF; ISO 37
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.15-0.35%, KM 08
 Oil32.2-34.1%, KM 05
 Polystyrene29.2-32.2%, KM 03
Styrene/Rubber Ratio31/69

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Kibiton® PB-511 SBC
Kraton® D1184 A (SBS) Branched Block Copolymer
Chi Mei Kibiton® PB-587 SBC
Chi Mei Kibiton® PB-585R SBC
Dynasol Calprene® 411 Thermoplastic Rubber SBS Dry

PKRA9846 / 132745

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.