MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parson Adhesives SONLOCK™ 3243 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive

Material Notes: SONLOK 3243 is a fast curing, medium strength anaerobic thread locking compound for bonding and sealing threads, and retaining of cylindrical parts. SONLOK 3243 is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.

Applications:

  • Ideal for less active material such as stainless steel, and plated parts.
  • Ideal for fasteners between ¼” and ¾” (6 to 20 mm) diameters.
  • Locks and seals threaded joints-nuts, screws, and studs with improved oil resistance.
  • Meets Military specifications: MIL-S-46163 Type II Grade N; MIL-S-22473E Letter Grade CVV

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Brookfield Viscosity 2250 cPRVT, Spindle 3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 1000 psiSteel Pins & Collars; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 3.00 hourFunctional
 10.0 - 12.0 minHandling
 24.0 hourFull
Shelf Life 24.0 Month
 
Descriptive Properties
ColorBlue
CompositionDimethacrylate Ester
Diameter<0.2 mmThread/Gap Filling
Initial Strength Retained (%)100Ethanol for 500 hrs at 22°C
 100Ethanol for 1000 hrs at 22°C
 100Gasoline for 500 hrs at 22°C
 100Gasoline for 1000 hrs at 22°C
 100Break Fluid for 500 hrs at 22°C
 100Break Fluid for 1000 hrs at 22°C
 80Water/Glycol for 1000 hrs at 87°C
 90Acetone for 1000 hrs at 22°C
 90Water/Glycol for 500 hrs at 87°C
 95Motor Oil for 500 hrs at 125°C
 95Motor Oil for 1000 hrs at 125°C
 95Acetone for 500 hrs at 22°C
Torque20 NmBreakaway, M10 steel nuts and bolts, ISO 10964
 24 NmBreakloose, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 24 NmMax Prevail, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 7 NmPrevail, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN016 / 186459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.