MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Koolkut® 8052B ISO Grade 22
Categories: Fluid; Lubricant

Material Notes: Koolkut 8052B is a light-colored, low-viscosity, chlorine-free tri-purpose oil formulated for use as a high-performance cutting oil, gear oil and hydraulic fluid in metalworking machines. Koolkut 8052B is formulated with fatty acids, polymers and a chlorine-free extreme-pressure additive package. The combination of extreme-pressure properties and good oiliness characteristics helps minimize cutting tool wear and ensure a good surface finish on the machined parts. Koolkut 8052B is transparent, allowing good observation of the machining operation. It is noncorrosive to copper and copper alloys and provides good rust protection for ferrous metals. The absence of chlorine ensures greater handling safety and safe disposal of waste oil. Koolkut 8052B is ideal for use in automatic screw machines that use one fluid to lubricate the cutting tool and workpiece, the machine gears, and the hydraulic pumps and motors. It also is suitable for use in lathes where mixing of the hydraulic fluid and cutting oil may occur. The performance capabilities of most cutting oils are greatly reduced when diluted with typical hydraulic oils. Using Koolkut 8052B as a lubricating oil and cutting oil avoids this problem.

Applications: Koolkut 8052B is recommended for light- to heavy-duty machining of ferrous and non-ferrous metals. Typical applications include:

  • Boring
  • Planing
  • Broaching
  • Sawing
  • Drilling
  • Screw machining
  • Gear hobbing
  • Shaping
  • Grinding
  • Tapping
  • Milling
Koolkut 8052B is suitable for machining a wide variety of metals ranging from steels with a machinability rating of 90%, to metals such as inconel, monel and titanium with machinability ratings below 50%.

Features/Benefit:

  • Tri-purpose cutting oil, gear oil and hydraulic oil
  • Helps extend cutting tool life
  • Good surface finish
  • Good rust protection
  • Noncorrosive to copper and copper alloys
  • Chlorine-free for reduced environmental impact
  • Transparent for good visibility of the machining operation

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.901 g/cc
Density 7.50 lb/gal
Viscosity Measurement 40Index
Saybolt Viscosity at 100°F 116 SUS
Saybolt Viscosity at 210°F 39.4 SUS
Kinematic Viscosity at 40°C (104°F) 22 cSt
Kinematic Viscosity at 100°C (212°F) 3.9 cSt
ASTM Color 3.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 3.5[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -34.0 °C
Flash Point 177 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.10 %
Sulfur, S 0.30 %
 
Descriptive Properties
Composition8%Fatty Oil
Copper Corrosion1bASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Titanium Ti-5Al-2.5Sn, ELI, Annealed
Titanium Beta-21S (Grade 21)

WCON5261 / 198514

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.