MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Multiflex™ A6221 CUV Styrenic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Thermoplastic Elastomer based Styrenic

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Melt Flow 76.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
76.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
cm³/10min Volumetric; ISO 1133
Spiral Flow 59.0 cm23.2 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 4.00 MPa580 psiISO 527-1/-2 or ISO 37
Elongation at Break >= 300 %>= 300 %ISO 527-1/-2 or ISO 37
Tear Strength 22.0 kN/m126 pliparallel; ISO 34-1
Compression Set 21 %
@Temperature 23.0 °C
21 %
@Temperature 73.4 °F
ISO 815
 65 %
@Temperature 70.0 °C,
Time 86400 sec
65 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °FOptimum, Injection
Mold Temperature 35.0 °C95.0 °FOptimum, Injection
 25.0 - 45.0 °C77.0 - 113 °FInjection
Drying Temperature 70.0 °C158 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 
Descriptive Properties
CompatibilityPolyolefins
Drying RecommendednoInjection
Injection speedMedium
PolymerTPS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9314 / 254363

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.