MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sodium Chloride, NaCl (Halite)
Categories: Ceramic; Halide

Material Notes: Colorless cubic crystals.

Critical relative humidity for stability is 76%. Crystallization Pressure for C/CS = 2 is 554 atm at 0°C. Crystallization Pressure for C/CS = 2 is 654 atm at 50°C.Crystallization Pressure for C/CS = 10 is 1845 atm at 0°C. Crystallization Pressure for C/CS = 10 is 2190 atm at 50°C.Crystallization Pressure for C/CS = 50 is 3135 atm at 0°C. Crystallization Pressure for C/CS = 50 is 3737 atm at 50°C.

Property values are typical of naturally occurring Halite (NaCl). Actual property values will vary from sample to sample.

Key Words: NaCl, Rock Salt
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.17 g/cc
a Lattice Constant 5.6402 Å
Formula Units/Cell (Z) 4
Molecular Weight 58.443 g/mol
 
Chemical PropertiesOriginal ValueComments
Molar Volume 28 cc/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.0
Compressive Strength 27.0 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1e+05 - 1.00e+6 ohm-cm
Magnetic Susceptibility -0.0000302cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 481.8 J/g
CTE, linear 40.0 µm/m-°C
Specific Heat Capacity 0.849 - 0.900 J/g-°C
Thermal Conductivity 3.13 - 3.87 W/m-K
Melting Point 800.7 °C
Boiling Point 1465 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.544
@Wavelength 589.3 nm
η, Na
 
Descriptive Properties
CAS Number7647-14-5
Crystal StructureCubicRock salt

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mateck Sodium Chloride (NaCl)
Hydrogen, H2
Potassium Chloride, KCl (Sylvite)
American Rock Elm Wood
Mateck Potassium Chloride (KCl)

EINOR0761 / 3893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.