MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Crastin® SC193 NC010 PBT+SAN-GF30  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); SAN Polymer

Material Notes: 30% Glass Reinforced Polybutylene Terephthalate Blend Developed for Healthcare Industry

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
Melt Density 1.28 g/cc
@Temperature >=225 °C
Water Absorption 0.70 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.250 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4, 2577
Melt Flow 13.3 g/10 min
@Load 5.00 kg,
Temperature 250 °C
from MVR and melt density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 9500 MPaISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 66.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 9000 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 7300 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 36.0 kV/mmIEC 60243-1
Dissipation Factor 0.0030
@Frequency 100 Hz
IEC 62631-2-1
 0.017
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 550 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 1.90 J/g-°C
@Temperature >=225 °C
Melt
Thermal Conductivity 0.260 W/m-K
@Temperature >=225 °C
Melt
Melting Point 225 °C10°C/min; ISO 11357-1/-3
 225 °C10°C/min; ISO 11357-1/-3
 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 180 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 97.0 °CISO 75-1/-2
Vicat Softening Point 150 °C50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 120 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 6.00 mm
IEC 60695-11-10
Oxygen Index 19 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CInjection Optimum
 240 - 260 °CInjection
 250 °CInjection Optimum
 240 - 260 °CInjection
 <= 260 °CInjection
Mold Temperature 30.0 - 130 °CInjection
 80.0 °CInjection Optimum
 30.0 - 130 °CInjection
 80.0 °CInjection Optimum
 <= 130 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.040 %Injection
Hold Pressure 60.0 MPaInjection
 
Descriptive Properties
Back pressureAs low as possibleInjection
Delivery formPellets
Drying RecommendedyesInjection
Hold pressure time (s/mm)3Injection
Part Marking CodePBT+SAN-GF30ISO 11469
ProcessingInjection Molding
Resin IdentificationPBT+SAN-GF30ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Crastin® LW9330 NC010 PBT+SAN-GF30
Celanese Crastin® LW9330 BK851 PBT+SAN-GF30
Celanese Crastin® LW9030 NC010 PBT+ASA-GF30
Celanese Crastin® SK602 BK851 PBT-GF15
Celanese Crastin® SC164 NC010 PBT

PDSX5051c / 230532

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.