MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer, 80 Shore A  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene

Material Notes: Styrene-Butadiene Copolymer

Description: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides excellent mechanical and elastic properties to compound.

Applications: Thanks to its high molecular weight Finaprene® 411x is designed for the compounding industry. This crumb shape, along with the high molecular weight confer a quick and important oil absorption capacity to the polymer and lead tot eh production of economical compounds while keeping good mechanical properties.

Additional Notes:
Oil Content: 5 phr; Finaprene 1010

Data provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccFinaprene 2602 Test
Viscosity Measure 25 cStToluene Solution; Finaprene 1008 Test
 
Chemical PropertiesOriginal ValueComments
Styrene Content 31 %Finaprene 1004 Test
Butadiene Content 69 %Finaprene 1004 Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Finaprene 1505 Test
Tensile Strength, Ultimate 15.0 MPaASTM D638
Elongation at Break 700 %ASTM D638

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1200-80A  Polyurethane Thermoplastic Elastomer (TPU) 80 Shore A
RTP Company RTP 1205-80A  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 30% - 80 Shore A
3M Scotchcast™ 2131 Flame-Retardant Compound
RTP Company RTP 1200-80A TFE 15  Polyurethane Thermoplastic Elastomer (TPU) PTFE 15% - 80 Shore A
Total Finaprene® 409 Styrene-Butadiene TPE Copolymer

PFINAP004 / 38591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.