Hydrin C2000L is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000L typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions. Low viscosity version of Hydrin C2000. |