MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kureha Krefine® ESD PEEK EKH SS07
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Krefine® ESD PEEK EKH SS07 offers surface resistivity in the 10^6 to 10^8 ohm/square range. Krefine® ESD PEEK is available in various grades for exact surface resistivity requirements, ranging from 10^6 to 10^12. The carbon filler is extremely homogeneous throughout the material. This means no conductive or insulative hot or cold spots. The milled carbon fiber filler is also much easier to machine than conventional carbon fillers. The carbon filler is extremely clean. You will not experience the sloughing which has typically been associated with carbon powder. The complete Krefine® PEEK product line includes the following grades:
  • EKH-SS07 surface resistivity in the 10^6 to 10^8 ohm/square range
  • EKH-SS09 surface resistivity in the 10^8 to 10^10 ohm/square range
  • EKH-SS11 surface resistivity in the 10^10 to 10^12 ohm/square range
  • EKH-SS12 surface resistivity in the 10^11 to 10^12 ohm/square range
Key Properties:
  • Ability to control respective resistivities within 10 to the first power in the range of 10^6-10^12 ohms/sq
  • Homogeneous surface and volume resistivity
  • Low metal contamination
  • Low out-gassing
  • Chemical Resistance
  • Weak acid; acetic acid, benzoic acid, hydrochloric acid surface acid - Acceptable
  • Weak alkalis; dilute ammonia, potassium hydroxide, sodium hydroxide - Acceptable
  • Strong alkalis; strong ammonia, potassium hydroxide, sodium hydroxide - Acceptable
  • Hydrocarbons – aromatic; benzene toluene, naphthalene – Acceptable
  • Hydrocarbons- aliphatic; heptane, gasoline, hexane, iso-octane, grease- Acceptable
  • Aldehydes and Ketones; acetone, methyl ethyl ketone, N-methyl-2-pyrrolidone - Acceptable
  • Esters; aliphatic esters, amyl acetate, dimenthyl phthalate - Acceptable
  • Chlorinated solvent; methylene chloride, chloroform – Acceptable
  • Alcohols; methanol, ethanol, glycols, benzyl alcohol – Acceptable
Limitations:
  • Chemical Resistance
  • Strong acid; conc. Hydrochloric, nitric acid, sulfuric acid
Applications:
  • Burn-In Sockets
  • Chip Carriers
  • FOUP
  • HADD related parts
  • IC and HGA trays
  • IC Test Socket
  • Liquid crystal display cassettes
  • Liquid crystal display related parts
  • Slider Tray
  • Spin chuck
  • Storage trays and bins
  • Wafer Carriers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Water Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
Immersion; ASTM D570
Water Absorption at Saturation 0.300 %0.300 %Immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 125125ASTM D785
Tensile Strength 140 MPa20300 psiASTM D638
Elongation at Break 2.50 %2.50 %ASTM D638
Flexural Strength 200 MPa29000 psiASTM D790
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Compressive Strength 180 MPa26100 psiASTM D695
Compressive Modulus 9.00 GPa1310 ksiASTM D695
Izod Impact, Notched 0.299 J/cm0.560 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+6 - 1.00e+8 ohm1.00e+6 - 1.00e+8 ohmASTM D257
Dielectric Constant 7.90
@Frequency 1.00e+6 Hz
7.90
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C15.0 µin/in-°FASTM D695
Melting Point 304 °C579 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 305 °C581 °FASTM D648
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKUREHA80 / 326949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.