MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraiburg TPE THERMOLAST® K TP7HPG Thermoplastic Elastomer (EX/UV Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The EX/UV series is a material solution for extrusion applications with increased requirements for UV resistance. The compounds are available in black, grey and natural colors. Natural color variants can be colored in many different ways. Some compounds of the series are approved according to RAL GZ 716 and/or CSTB QB36.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Grey
  • Natural
  • Black
Typical applications:
  • Door and window seals for outdoor applications
  • Distance profiles
  • Edge guards
Material advantages:
  • UV and weathering resistance
  • Adhesion to PP
  • Halogen-free (according to IEC 61249-2-21)
  • Resistance to acrylic paints
  • Weldable (Infrared & Mirror)
  • No interaction with other materials (e.g. PVC-U, PC, PMMA)
  • In-process recycling possible
  • Alternative material to PVC-P

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6969DIN ISO 48-4
Tensile Strength 10.0 MPa1450 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 750 %750 %200 mm/min; DIN 53504/ISO 37
Compression Set  21 %
@Temperature 23.0 °C,
Time 259000 sec
21 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 55 %
@Temperature 70.0 °C,
Time 86400 sec
55 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8116 / 308780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.