- Available in North America
- Filler: Mineral, 40% Filler by Weight
- Additive: Heat Stabilizer and Lubricant
- Features: Lubricated, Low Warpage and Heat Stabilized
- RoHS Compliant
- Form: Pellets
- Processing Method: Injection Molding
- Color: Black
Information provided by Ravago. |