MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
JIS SKH51 Molybdenum High Speed Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel

Key Words: JIS G4403(83) SKH51, SKH 51, SKH-51; Comparable to SKH9 (obsolete), AISI M2 Tool Steel, UNS T11302
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.14 g/cc(AISI M2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 255Bar/Forging Annealed
Modulus of Elasticity 207 GPa(AISI M2)
Charpy Impact 23.0 - 28.0 ft-lbAustenitized and Tempered
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000540 ohm-cm(AISI M2)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 - 100 °C
(AISI M2)
 11.7 µm/m-°C
@Temperature 20.0 - 200 °C
(AISI M2)
 12.2 µm/m-°C
@Temperature 20.0 - 300 °C
(AISI M2)
 12.4 µm/m-°C
@Temperature 20.0 - 400 °C
(AISI M2)
 12.7 µm/m-°C
@Temperature 20.0 - 500 °C
(AISI M2)
 12.9 µm/m-°C
@Temperature 20.0 - 700 °C
(AISI M2)
 13.0 µm/m-°C
@Temperature 20.0 - 600 °C
(AISI M2)
Specific Heat Capacity 0.460 J/g-°C(AISI M2)
Thermal Conductivity 19.0 W/m-K(AISI M2)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.80 - 0.90 %
Chromium, Cr 3.8 - 4.5 %
Copper, Cu <= 0.25 %
Iron, Fe 79 - 83.8 %As Balance
Manganese, Mn <= 0.40 %
Molybdenum, Mo 4.5 - 5.5 %
Nickel, Ni <= 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.030 %
Tungsten, W 5.5 - 6.7 %
Vanadium, V 1.6 - 2.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A283 Steel, grade D
JIS S45C Steel, Normalized
AISI Type P20 Mold Steel (UNS T51620)
JIS S45C Steel, Tempered
JIS SKS3 Oil-hardening Cold Work Tool Steel

MSTZJSKH51 / 231080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.