MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plastcom SLOVAMID® 6/66C GF 30 HI Polyamide 6/66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: PA 6/66 co polyamide with the content of thermoplastic elastomeric. Impacted, for moldings with high toughness even at low temperatures, suitable for external use, e.g.. ski shoes, sports and safety helmets, protection ledges of the car-doors. Delivered in natural and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inSTN EN ISO 294-4
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 527 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa23200 psiSTN EN ISO 527-2
Elongation at Break 4.0 %4.0 %STN EN ISO 527-2
Tensile Modulus 9.50 GPa1380 ksiSTN EN ISO 527-2
Flexural Strength 195 MPa28300 psiSTN EN ISO 178
Flexural Modulus 7.40 GPa1070 ksiSTN EN ISO 178
Charpy Impact Unnotched  8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 8.00 J/cm²
@Temperature -20.0 °C
38.1 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 205 °C401 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.15 %0.15 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN912 / 282504

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.