MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Weifang Tianrui Chemical LPn125 Acrylic Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Introduction: The series is based on acrylic polymer with functional organic materials and inorganic nanomaterials into complex mix of PVC processing modifier. Manly used for PVC profile, pipe.

Characteristics and Application: In the hard PVC products by adding a small amount of (1.5-2.0) the series of processing aid, the promotion of PVC will be able to gel and improve the melt strength of the melt, obviously improve the physical properties and surface finish of products.

Information provided by Weifang Tianrui Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.5 %<= 1.5 %
Apparent Bulk Density 0.350 - 0.650 g/cc0.0126 - 0.0235 lb/inĀ³
Particle Mesh Size 40 Mesh40 Mesh>98% Granularity (percent of pass)
Viscosity Measurement 3.0 - 5.03.0 - 5.0Intrinsic Viscosity(?)
 
Descriptive Properties
AppearanceWhite freely flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEIFTC023 / 320536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.