MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® MonoPlus M 800 OH Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus M 800 OH is a strongly basic, gelular anion exchange resin (type I) with beads of uniform size (monodisperse) base on a styrene-divinylbenzene copolymer, in a highly regenerated form, designed for all demineralization applications. The monodisperse beads have high chemical and osmotic stability. The extremely high monodispersity (uniformity coefficient max. 1.1) and very low fines content of max. 0.1% (<0.350 mm) result in particularly low pressure losses compared with standard resins. Lewatit MonoPlus M 800 OH is especially suitable for:
  • conventional mixed bed application in combination with Lewatit® MonoPlus S 200 KR or Lewatit® MonoPlus S 108 H
  • polishing using the Lewati Multistep System
  • condensate polishing in combination with Lewatit® MonoPlus S 200 KR or Lewatit® MonoPlus SP 112 H
Lewatit MonoPlus M 800 OH adds special features to the resin bed:
  • high exchange flow rates during regeneration and loading
  • good utilization of the total capacity
  • low rinse water requirement
  • homogeneous throughput of regenerants, water and solutions, resulting in a homogenous operating zone
  • virtually linear pressure drop gradient across the entire bed depth, allowing operation with higher bed depths
  • good separation of the components in mixed bed applications

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.680 g/cc
Density 1.07 g/cc
Bead Size 0.590 - 0.690 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceLight amber, translucent
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess LEWATIT® MonoPlus S 215 KR Cation Exchange Resin

PLANY8782 / 209174

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.