MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes 556® alloy, bar, after 1000 hours at 650°C (1200°F)
Categories: Metal; Superalloy; Iron Base

Material Notes: Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists corrosion by molten chloride salts and is resistant to corrosion from molten zinc. Excellent forming and welding characteristics. Applications include tubing and structural members in municipal and industrial waste incinerators, rotary calciners and kilns for minerals processing, and non-rotating components in land-based gas turbines burning low-grade fuels; carbon regenerators, and in processes involving high-sulfur petroleum feedstocks; widely used for hot-dip galvanizing fixtures, spinners, and baskets, high speed furnace fans, air preheaters of diesel engines, the inner covers of coil annealing furnaces, and various high temperature applications in the aerospace industry.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS R30556, AMS 5874, AMS 5877, AMS 5831
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.23 g/ccat RT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 830 MPa
Tensile Strength, Yield 410 MPa
@Strain 0.2 %
Elongation at Break 36 %in 50.8 mm
Modulus of Elasticity 205 GPaRT
 138 GPa
@Temperature 1000 °C
 143 GPa
@Temperature 900 °C
 148 GPa
@Temperature 800 °C
 155 GPa
@Temperature 700 °C
 164 GPa
@Temperature 600 °C
 172 GPa
@Temperature 500 °C
 179 GPa
@Temperature 400 °C
 187 GPa
@Temperature 300 °C
 195 GPa
@Temperature 200 °C
 200 GPa
@Temperature 100 °C
Charpy Impact 240 JSamples did not break. Average of 4 or more tests.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000952 ohm-cmRT
 0.0000986 ohm-cm
@Temperature 100 °C
 0.0001026 ohm-cm
@Temperature 200 °C
 0.0001065 ohm-cm
@Temperature 300 °C
 0.0001095 ohm-cm
@Temperature 400 °C
 0.0001125 ohm-cm
@Temperature 500 °C
 0.0001151 ohm-cm
@Temperature 600 °C
 0.0001172 ohm-cm
@Temperature 700 °C
 0.000119 ohm-cm
@Temperature 800 °C
 0.0001207 ohm-cm
@Temperature 900 °C
 0.0001223 ohm-cm
@Temperature 1000 °C
 0.0001237 ohm-cm
@Temperature 1100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.7 µm/m-°C
@Temperature 25.0 - 100 °C
 14.9 µm/m-°C
@Temperature 25.0 - 200 °C
 15.1 µm/m-°C
@Temperature 25.0 - 300 °C
 15.4 µm/m-°C
@Temperature 25.0 - 400 °C
 15.7 µm/m-°C
@Temperature 25.0 - 500 °C
 16.1 µm/m-°C
@Temperature 25.0 - 600 °C
 16.4 µm/m-°C
@Temperature 25.0 - 700 °C
 16.7 µm/m-°C
@Temperature 25.0 - 800 °C
 17.0 µm/m-°C
@Temperature 25.0 - 900 °C
 17.1 µm/m-°C
@Temperature 25.0 - 1000 °C
Specific Heat Capacity 0.464 J/g-°CRT
 0.475 J/g-°C
@Temperature 100 °C
 0.493 J/g-°C
@Temperature 200 °C
 0.508 J/g-°C
@Temperature 300 °C
 0.523 J/g-°C
@Temperature 400 °C
 0.538 J/g-°C
@Temperature 500 °C
 0.552 J/g-°C
@Temperature 600 °C
 0.561 J/g-°C
@Temperature 700 °C
 0.570 J/g-°C
@Temperature 800 °C
 0.595 J/g-°C
@Temperature 900 °C
 0.618 J/g-°C
@Temperature 1000 °C
 0.638 J/g-°C
@Temperature 1100 °C
Thermal Conductivity 11.1 W/m-KRT
 13.1 W/m-K
@Temperature 100 °C
 15.4 W/m-K
@Temperature 200 °C
 17.3 W/m-K
@Temperature 300 °C
 19.0 W/m-K
@Temperature 400 °C
 20.8 W/m-K
@Temperature 500 °C
 22.4 W/m-K
@Temperature 600 °C
 24.0 W/m-K
@Temperature 700 °C
 25.5 W/m-K
@Temperature 800 °C
 27.2 W/m-K
@Temperature 900 °C
 28.9 W/m-K
@Temperature 1000 °C
 30.4 W/m-K
@Temperature 1100 °C
Melting Point 1330 - 1415 °C
Solidus 1330 °C
Liquidus 1415 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.20 %
Carbon, C 0.10 %
Chromium, Cr 22 %
Cobalt, Co 18 %
Iron, Fe 31 %As remainder
Lanthanum, La 0.020 %
Manganese, Mn 1.0 %
Molybdenum, Mo 3.0 %
Nickel, Ni 20 %
Nitrogen, N 0.20 %
Silicon, Si 0.40 %
Tantalum, Ta 0.60 %
Tungsten, W 2.5 %
Zirconium, Zr 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Haynes 556® alloy, sheet after 1000 hours at 648°C
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Special Metals INCONEL® Alloy 625
Haynes 556® alloy, bar, after 8000 hours at 650°C (1200°F)

NH55AP / 16670

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.