MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shandong Rike Chemical ACM-1 PVC Impact Modifier ACM Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: For overcoming the shortcomings of plasticizers and CPE, this impact modifier ACM which as a copolymer of HDPE and acrylic acid was developed. ACM not only has the basic feature of CPE, but has higher impact strength and lower glass temperature compared to CPE, so its impact modification effect is more evident than CPE. Besides, ACM can effectively improve the weather-resistance of PVC products.

Application

The application method of ACM is the same as that of CPE. In processing, electric current and torque of extruders may have a slight decline and it may be eliminated through adjusting lubricant agent in the ingredients.

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Unnotched (ISO) 17.9 kJ/m²
@Temperature 0.000 °C
Phr = 0
 19.8 kJ/m²
@Temperature 23.0 °C
Phr = 0
 20.8 kJ/m²
@Temperature 0.000 °C
Phr = 5
 23.0 kJ/m²
@Temperature 0.000 °C
Phr = 8
 25.0 kJ/m²
@Temperature 23.0 °C
Phr = 5
 26.2 kJ/m²
@Temperature 23.0 °C
Phr = 8
 
Descriptive Properties
Balance Torque (N-m)29.810 Phr
 29.98 Phr
 30.35 Phr
Fusion Temperature (°C)1788 Phr
 17810 Phr
 1795 Phr
Fusion Time (s)20010 Phr
 2108 Phr
 2345 Phr
Torque (N-m)24.9-32.75 Phr
 25.0-32.08 Phr
 25.4-30.910 Phr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATG s.r.l. ACM Polyacrylic Rubber
Aluminum 3003-H14
Wacker Vinnol® E 15/40 A TF Vinyl Chloride Copolymer
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Aluminum 3003-H112

PSHAN075 / 103465

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.