MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fainplast Compounds Ethylplus 613 HGI /4 Cable Grade Polyethylene - Foam Insulation
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Suitable for the production of solid and foam insulation for data, telecommunication, coaxial and other signal cables or in the production of sheathing for outdoor and direct burial cables. Description: Gas inj. exp. HDPE for dielectric.

Information provided by Fainplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ISO 1183
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 140 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 284 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 56
@Time 15.0 sec
56
@Time 0.00417 hour
ISO 868
Tensile Strength at Break >= 18.0 MPa>= 2610 psi250 mm/min; ISO 527
Elongation at Break >= 300 %>= 300 %250mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 2.00e+16 ohm-cm
@Temperature 20.0 °C
>= 2.00e+16 ohm-cm
@Temperature 68.0 °F
Alternating Polarity Method; ASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFAIN9875 / 282374

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.