MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the ability to retain their original color and state.

Applications:

  • Outdoor furniture
  • Automotive
  • Appliances

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Filler Content 20 %20 %ASTM D2584
Linear Mold Shrinkage 0.012 cm/cm
@Thickness 1.59 mm
0.012 in/in
@Thickness 0.0625 in
ASTM D955
Melt Flow 16 - 20 g/10 min16 - 20 g/10 min230/2.16; May be specified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8787ASTM D785
Tensile Strength at Break 27.6 MPa4000 psiASTM D638
Flexural Modulus 2.00 GPa290 ksiTangent; ASTM D790
Izod Impact, Notched 0.721 J/cm1.35 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 6.67 J/cm12.5 ft-lb/inAt 73°F; ASTM D256
Gardner Impact 5.197 J3.833 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
DuPont Mobility and Materials Neoprene TRT Polychloroprene Rubber
Plastics Group Polifil® RMT-10 10% Talc-Reinforced Polypropylene, High Impact
Plastics Group Polifil® RMT-40V 40% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene

PPOLI008 / 56912

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.