MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Copper-Zinc-Lead Alloy (Leaded Brass)

Finished product available in shapes.
Chicago Extruded Metal temper codes: H01, H02

Information provided by Chicago Extruded Metals

Key Words: CDA 385, ASTM B455
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6565
Tensile Strength 414 MPa60000 psi
Tensile Strength, Yield 138 MPa20000 psi
Elongation at Break 30 %30 %
Machinability 90 %90 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000615 ohm-cm0.00000615 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 123 W/m-K852 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 55 - 59 %55 - 59 %
Iron, Fe 0.35 %0.35 %
Lead, Pb 2.5 - 3.5 %2.5 - 3.5 %
Other, total 0.50 %0.50 %
Zinc, Zn 36.65 - 41.65 %36.65 - 41.65 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Architectural Bronze, UNS C38500
Extra-high-leaded brass, UNS C35600
Mueller Alloy 3850 Architectural Brass (UNS C38500)
Leaded Yellow Brass, UNS C85800, Copper Casting Alloy, Die Castings

NCHICA915 / 147634

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.