MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NuSil CV-2566 Silicone, Two Part Adhesive and Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Two Part Adhesive and Sealant

Comments: Pourable RTV Cure

Cure system: Alkoxy

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/cc
Viscosity 55000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55
Tensile Strength at Break 6.40 MPa
Elongation at Break 150 %
Shear Strength 4.00 MPaLap, Primed with SP-120
Tear Strength 40.0 pli
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 825 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 330 µm/m-°C
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 25.0 °C
Working Life 4.00 hour
 
Descriptive Properties
ColorRust
Mix Ratio100:0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond MasterSil 151AO Thermally Conductive Silicone System
Master Bond MasterSil 151 Two Component Low Viscosity Silicone Compound
Dow Q2-7566 ADHESIVE
Momentive Performance Materials RTV566 Silicone Rubber Compound for Low Outgassing Applications
NuSil CV-2568 Silicone, Two Part Adhesive and Sealant

PNUSIL171 / 141895

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.