Uncured silicone rubber with a minimum thickness of 0.0045 in. (0.11 mm) on 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.010 in ± 0.001 (0.25 mm ± 0.025). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 379.7 g/m² ± 30.52 (11.2 oz./yd.² ± 0.9). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |