Pro-fax 7823 fractional melt flow polypropylene copolymer is available in pellet form. This resin is typically used in extrusion applications and offers high melt strength and excellent impact resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax 7823. Availability: North America Application: Automotive Parts; Food Packaging Film; Raffia/Tapes/Strapping; Specialty Film; Underhood Market: Automotive; Compounding; Flexible Packaging; Textile Processing Method: Blown Film; Compounding; Extrusion Blow Molding; Sheet and Profile Extrusion; Thermoforming Attribute: Good Heat Aging Resistance; Good Impact Resistance; Good Melt Strength; Good Stiffness; Low Temperature Impact Resistance Information provided by LyondellBasell. |