MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Synthos SDH790 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characteristics: SDH series is a special kind of linear thermoplastic Polyurethane Elastomer, which is designed for TPU Hot-melt film. It exhibits good toughness, wear resistance, elasticity and excellent bonding strength for TPU, PVC, Nylon, Polyester, fabrics, leather etc.

Applications: Toe-Puffs& Counters, hot-melt adhesive films and tapes, Fabric coatings, Seam Sealing Tapes, shoe materials, high-end interlining, heat transfer printing industry, textile, etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
Tear Strength 110 kN/m628 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 155 °C311 °FASTM D6593
 
Processing PropertiesMetricEnglishComments
Cure Time 2.00 min0.0333 hourTack-free time
 
Descriptive Properties
Flow-beginning temperature140°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW127 / 320158

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.