MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

Saint-Gobain Meldin® 7021 Isostatically Molded Graphite Filled Polyimide
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Melidin® 7021 is a self-lubricating thermosetting polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best for high temperature bearing, seals, thrust washers, and low-wear applications.

Specification Qualifications:
Satisfies Type II, Class 1M for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide Resin
Satisfies Class 2, Form M for SAE AMS 3644G: Polyimide, Molded Rod, Bar and Tube, Plaque, and Formed Parts
Satisfies Type II, Class 1M for MIL-R-46198: Resin, Polyimide, Hot Pressed or Pressed and Sintered

Information provided by Saint-Gobain Performance Plastics

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 5050ASTM D785
Tensile Strength  37.9 MPa
@Temperature 260 °C
5500 psi
@Temperature 500 °F
ASTM D638
 65.5 MPa
@Temperature 23.0 °C
9500 psi
@Temperature 73.4 °F
ASTM D638
Elongation at Break  4.3 %
@Temperature 260 °C
4.3 %
@Temperature 500 °F
ASTM D638
 4.5 %
@Temperature 23.9 °C
4.5 %
@Temperature 75.0 °F
ASTM D638
Flexural Strength 108 MPa15600 psiASTM D790
Flexural Modulus 3.90 GPa566 ksiASTM D790
Compressive Yield Strength  26.2 MPa
@Strain 1 %
3800 psi
@Strain 1 %
ASTM D695
 133 MPa
@Strain 10 %
19300 psi
@Strain 10 %
ASTM D695
Compressive Modulus 2.30 GPa334 ksiASTM D695
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 11.0 kV/mm280 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C
@Temperature 23.9 - 260 °C
25.0 µin/in-°F
@Temperature 75.0 - 500 °F
ASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ 1000 IM Injection Molded Unfilled Polyetheretherketone
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide

PSTGQZ082 / 150620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.