System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical SEETEC BF315 LDPE
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
;
Low Density Polyethylene (LDPE), Film Grade
Material Notes:
Characteristics: Good Processability and Excellent Optical Properties
Applications: Masking film
CAS No. 9002-88-4
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.921
-
0.925
g/cc
0.921
-
0.925
g/cc
ASTM D1505
Melt Flow
0.80
-
1.2
g/10 min
@Load 2.61 kg,
Temperature 190 °C
0.80
-
1.2
g/10 min
@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
14.7
MPa
2130
psi
500mm/min; ASTM D638
Film Elongation at Break, MD
300 %
300 %
500 mm/min; ASTM D638
Film Elongation at Break, TD
550 %
550 %
500 mm/min; ASTM D638
Elongation at Break
600 %
600 %
500 mm/min; ASTM D638
2% Secant Modulus
1.25
GPa
181
ksi
500mm/min; ASTM D638
Elmendorf Tear Strength MD
450
g
450
g
ASTM D1922
Elmendorf Tear Strength TD
200
g
200
g
ASTM D1922
Dart Drop Test
75.0
g
0.165
lb
ASTM D1709
Film Tensile Strength at Break, MD
26.5
MPa
3840
psi
500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD
24.5
MPa
3550
psi
500mm/min, Ultimate; ASTM D638
Thermal Properties
Metric
English
Comments
Melting Point
105
°C
221
°F
10°C/min; ASTM D3418
Vicat Softening Point
94.0
°C
201
°F
ASTM D1525
Optical Properties
Metric
English
Comments
Haze
6.0 %
6.0 %
ASTM D1003
Gloss
95 %
95 %
45°; ASTM D2457
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical SEETEC BC500 LDPE
LyondellBasell Lupolen 5261Z Q456 POWDER High Density Polyethylene (HDPE), Pipe Grade
LG Chemical SEETEC BF500 LDPE
Versalis Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion
LG Chemical SEETEC BS500 LDPE
PLAY220 / 148230
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.