MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terluran® KR2910 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: Terluran® KR2910 acrylonitrile/butadiene/styrene copolymer (ABS) is a general purpose, extrusion grade resin with good impact resistance and processing characteristics. Terluran® KR2910 is intended for use as drain, waste and vent (DWV) applications.
ASTM D3965 Pipe and Fitting Cell Classification: Terluran® KR2910 Black 10009: 4-2-4-2-2; Terluran® KR2910 Natural: 4-3-4-2-2
Features: High toughness; Very high impact; Medium low; Great mechanical strength and rigidity; High impact at sub-zero temperatures
Applications: Extrusion; NSF/ANSI 14; Sewer and continuous waste

Availability: Latin America; North America

Features: General Purpose; Good Processability; Good Rigidity; Good Strength; High Impact Resistance; High Toughness; Low Temperature Impact Resistance; Medium Flow

Uses: General Purpose

Agency Ratings: ASTM D3965; NSF STD-14

Processing Method: Extrusion

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Water Absorption at Saturation 1.0 %ASTM D570
Linear Mold Shrinkage, Flow 0.00 - 0.010 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Film Tensile Strength at Yield, TD 5650 psiASTM D882
Tensile Strength, Yield 6240 psiASTM D638
Elongation at Break 3.5 %ASTM D638
Tensile Modulus 290000 psiASTM D638
Flexural Strength 9570 psiASTM D790
Flexural Modulus 297000 psiASTM D790
Izod Impact, Notched 2.20 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 3.40 ft-lb/in
@Temperature -17.8 °C
ASTM D256
 8.40 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 1.75 ft-lbASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 201 °FUnannealed; ASTM D648
 215 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 186 °FUnannealed; ASTM D648
 208 °FAnnealed; ASTM D648
Vicat Softening Point 201 °FISO 306/A50
 
Processing PropertiesOriginal ValueComments
Drying Temperature 160 - 180 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYS780 / 311473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.