MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plastcom SLOVAMID® 66 GF 45 HTS Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: PA66 for injection molding grade, reinforced with 45% glass fiber, heat stabilized, hydrolysis resistant, determined for injection molding of parts like oil pipes, parts in engine. Delivered in natural and black color.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inSTN EN ISO 294-4
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 527 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 210 MPa30500 psiSTN EN ISO 527-2
Elongation at Break 2.0 %2.0 %STN EN ISO 527-2
Tensile Modulus 14.8 GPa2150 ksiSTN EN ISO 527-2
Flexural Strength 265 MPa38400 psiSTN EN ISO 178
Flexural Modulus 11.25 GPa1632 ksiSTN EN ISO 178
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -20.0 °C
42.8 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  1.20 J/cm²
@Temperature -20.0 °C
5.71 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmSTN 34 6460
Surface Resistance 1.00e+14 ohm1.00e+14 ohmSTN 34 6460
Dielectric Strength 25.0 kV/mm635 kV/inSTN EN 60243-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 250 °C482 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.15 %0.15 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN928 / 282520

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.