MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

SABIC XENOY™ HX5600HP PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, Gamma and Steam sterilizable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Water Absorption 0.40 %0.40 %23°C/sat; ISO 62
Moisture Absorption 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Viscosity 260 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
260 cP
@Shear Rate 1500 1/s,
Temperature 500 °F
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0070 - 0.011 cm/cm
@Thickness 3.20 mm
0.0070 - 0.011 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  10 g/10 min
@Load 5.00 kg,
Temperature 250 °C
10 g/10 min
@Load 11.0 lb,
Temperature 482 °F
cm³/10 min; ISO 1133
 11 g/10 min
@Load 5.00 kg,
Temperature 250 °C
11 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psi50 mm/min; ASTM D638
 55.0 MPa7980 psi50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527
 50.0 MPa7250 psi50 mm/min; ASTM D638
Elongation at Break 100 %100 %50 mm/min; ISO 527
 150 %150 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.05 GPa297 ksi1mm/min; ISO 527
 2.10 GPa305 ksi5 mm/min; ASTM D638
Flexural Yield Strength 70.0 MPa10200 psi1.3 mm/min, 50 mm span; ASTM D790
 75.0 MPa10900 psi2 mm/min; ISO 178
Flexural Modulus 2.00 GPa290 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.05 GPa297 ksi2 mm/min; ISO 178
Izod Impact, Notched 7.50 J/cm14.1 ft-lb/inASTM D256
 6.00 J/cm
@Temperature -30.0 °C
11.2 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 55.0 kJ/m²26.2 ft-lb/in²80*10*4; ISO 180/1A
 25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 80.0 J59.0 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
176 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 123 °C253 °FRate B/120; ISO 306
 125 °C257 °FRate B/50; ASTM D1525
 125 °C257 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature
Nozzle Temperature 250 - 265 °C482 - 509 °FInjection Molding
Zone 1 230 - 250 °C446 - 482 °F
Zone 2 240 - 265 °C464 - 509 °F
Zone 3 250 - 270 °C482 - 518 °F
Melt Temperature 255 - 270 °C491 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 90.0 - 100 °C194 - 212 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10837 / 244304

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.