MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax RP323M Polypropylene Copolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Pro-fax RP323M is a barefoot polypropylene random copolymer available in pellet form. This resin is typically used in cast film packaging applications. Typical properties of cast film made with this resin are excellent clarity and gloss, as well as improved cold temperature impact resistance and broader heat seal range compared to homopolymer polypropylene. Applications: Bags & Pouches, Breathable Film, Film Wrap, Food Packaging Film, Heavy Duty Packaging, Hygiene Film, Peelable Film, Stationery Film, Stretch Wrap Film, Twist Wrap Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.8 MPa50mm/min; ASTM D638
Elongation at Yield 14 %ASTM D638
Flexural Modulus, 1% Secant 830 MPa1.3 in/min, Procedure A; ASTM D790
Izod Impact, Notched 64.0 J/m
@Temperature 23.0 °C
Method A; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °Cunannealed; ASTM D648
 
Descriptive Properties
Processing MethodCast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem 6D83G Polypropylene Random Copolymer
Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding
Total PPR 7425 Polypropylene, Injection Molding Grade
Total PPR 8473 Polypropylene, Film Extrusion Grade
Braskem RP650 Polypropylene Random Copolymer

PEQT8800 / 220434

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.