MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ EP-20 Epoxy Resion with Thermoset Hardener No. 66 System
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD Thermoset EP-20/66 epoxy system is a two-component, general purpose system for use in many applications including adhesive, laminating and electrical/electronic insulation. Handling and cured properties of the two-component epoxy system are dependent on the hardener used with Thermoset EP-20 epoxy resin.

Features: provides high bond strength for use as an adhesive to a variety of surfaces. Rigidity of bond may be varied depending on mix ratio. A 1:2 (resin to hardener, by weight) ratio will yield a relatively flexible bond; a 2:1 ratio will provide a rigid bond. provides a working life of over one hour; cures at room temperature or with mild elevated temperature.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccHardener
 1.17 g/ccEP-20 Component
Water Absorption 0.35 %
@Temperature 25.0 °C,
Time 86400 sec
cured
Viscosity 10000 cP
@Temperature 25.0 °C
Hardener; Spindle 5, 20 rpm
 13000 cP
@Temperature 25.0 °C
EP-20 Component
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85cured; ASTM D 2240
Tensile Strength 7500 psi
@Temperature 25.0 °C
cured
Elongation at Break 12 %cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Temperature 25.0 °C
cured
Dielectric Constant 3.7
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured
Dissipation Factor 0.016
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
mixed with EP-20 Epoxy Resin
Working Life 60.0 min
@Temperature 25.0 °C
Working life, with EP-20 Epoxy Resin
Shelf Life 24.0 Month
@Temperature 25.0 °C
Hardener. From date of manufacture in original, unopened container
 24.0 Month
@Temperature 15.0 - 35.0 °C
EP-20 Component. From date of manufacture in original, unopened container
 
Descriptive Properties
AppearanceAmber LiquidHardener 67
 Black LiquidEP-20
Mix Ratio100 to 50by weight, EP-20 Epoxy Resin to Hardener
 100 to 60by volume, EP-20 Epoxy Resin to Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant
Resinlab® EP1026 Black Epoxy Adhesive

PLORD9167 / 232555

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.