MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Baymod® PU-A Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Baymod® PU-A is a plasticizing polymer for improving the resistance of PVC and POM to oil, grease, solvents and abrasion.

Chemical composition: aliphatic polyester urethane

Applications: Baymod® PU-A is a very flexible aliphatic polyester urethane developed especially for processing with PVC and POM.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 6.0 - 26 cP6.0 - 26 cP5% in dimethylformamide; DIN 53015
Melt Flow 10 - 35 g/10 min
@Load 5.00 kg,
Temperature 180 °C
10 - 35 g/10 min
@Load 11.0 lb,
Temperature 356 °F
DIN EN ISO 60
Ash <= 1.0 %<= 1.0 %
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 5042 Polypropylene, Homopolymer
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Chang Chun Plastic PBT1100L General Purpose PBT
Avient Maxxam® FR PP FR 7D31 Flame Retardant Polypropylene, Impact Modified

PLANY8388 / 208781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.