MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon CP-RC-3918 Silicone Bulk Compound
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes:

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³Silicone Property; Arlon SQA-TMS-024
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4646Silicone Property; ASTM D2240
Tensile Strength 8.584 MPa1245 psiSilicone Property; ASTM D412
Elongation at Break 565 %565 %Silicone Property; ASTM D412
Tear Strength 17.5 kN/m100 pliSilicone Property; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Post Cure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 21.1 °C
6.00 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
Covestro Baybond® PU 406 Polyurethane
Covestro Baybond® PU 330 Polyester Urethane Polymer
CHT Group SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber

PARL9829 / 148982

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.