MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. Typical applications include heavy duty switch gear, connectors, and commutators.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.850 g/ccASTM D1895
Density 1.80 g/ccASTM D792
Water Absorption 0.050 %ASTM D570
Linear Mold Shrinkage 0.0025 cm/cmASTM D6289
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 69.0 MPaASTM D638
Tensile Modulus 17.2 GPaASTM D638
Flexural Strength 103 MPaASTM D790
Compressive Strength 241 MPaASTM D695
Izod Impact, Notched 37.4 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 4.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.8 kV/mmstep-by-step; ASTM D149
 17.7 kV/mmshort time; ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °CUL Temperature Index; at 3.0 mm
Deflection Temperature at 1.8 MPa (264 psi) 204 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 V-0
@Thickness 6.00 mm
 
Descriptive Properties
ColorBlack
Molding MethodCompression

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade

P90X933 / 142708

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.