MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vikas Ecotech ATH-100 Flame Retardant
Categories: Other Engineering Material

Material Notes: Product Description: Aluminum Trihydrate (ATH) is a flame retardant and smoke suppressant & an economical resin extender.

Characteristics & Usages: ATH is the most popular low smoke, non-toxic additive, it is a common replacement for antimony based complex additives in vinyl applications, it is also recommend for PVC, latex, neoprene foam systems, rubbers wire & cable insulations, vinyl walls & flooring coverings and Epoxies etc. Aluminum Trihydraet acts as a flame retardant and smoke suppressant. Its thermodynamic properties, endothermic dehydration cools the plastic & rubber parts and dilutes the combustible gases with water vapor that is generated in case of fire.

Information provided by Vikas Ecotech LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.40 g/cc2.40 g/cc
Particle Size 9.0 - 11 µm9.0 - 11 µm
Maximum Moisture Content 0.500.50
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 65 %>= 65 %
Fe2O3 <= 0.010 %<= 0.010 %
Loss on Ignition(%) 34.5 %34.5 %
Na2O <= 0.010 %<= 0.010 %
SiO2 <= 0.010 %<= 0.010 %
TiO2 <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICAS007 / 285420

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.