MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

97Sn-3Ag Tin-Silver Solder, ISO/DIS 9453 Alloy 29
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: Solder is the largest use for tin in the U.S. Tin promotes adhesion to many base metals. This particular alloy is used as a solder in electrical and high temperature applications.

Composition reported per ISO/DIS 9453.

Key Words: Tin Alloys
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.41 g/cc0.268 lb/in³Alloy 28
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 - 230 °C430 - 446 °F
Solidus 221 °C430 °F
Liquidus 230 °C446 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.001 %0.001 %
Antimony, Sb 0.10 %0.10 %
Arsenic, As 0.03 %0.03 %
Bismuth, Bi 0.10 %0.10 %
Cadmium, Cd 0.005 %0.005 %
Copper, Cu 0.10 %0.10 %
Indium, In 0.05 %0.05 %
Iron, Fe 0.02 %0.02 %
Lead, Pb 0.10 %0.10 %
Silver, Ag 3.0 - 3.5 %3.0 - 3.5 %
Tin, Sn 95.99 - 96.49 %95.99 - 96.49 %as balance
 97 %97 %Nominal
Zinc, Zn 0.001 %0.001 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
96Sn-4Ag Tin-Silver Solder, ASTM Class 96TS, ISO/DIS 9453 Alloy 28
AIM 96.5Sn/3.5Ag Solder for Photonic Packaging
Tin-Silver Solder (95Sn-5Ag), ASTM B 32 Grade Sn95
Eutectic Solder (63Sn-37Pb) - ASTM B 32 Grade Sn63
68.4Pb-30Sn-1.6Sb Tin-Lead-Antimony Solder, ASTM Class 30C

MLSS97 / 178192

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.