MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LX9002 | PA12 Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Plasticized, heat- and light- stabilized polyamide 12 compound VESTAMID LX9002 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of multilayer tubing 2030 and 2040 developed by Evonik Degussa GmbH. VESTAMID LX9002 is characterized by easy processing as well as by a high impact strength at low temperatures. VESTAMID LX9002 is recommended in order to attain an excellent bonding with DYFLOR X7394. VESTAMID LX9002 is supplied as cylindrical pellets, ready for use, in moisture-proof bags. It has to be noticed that material data measured on test specimens, do not provide sufficient information to draw conclusions on the final performance of the resin when used in a multilayer tubing. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527
Tensile Strength, Yield 27.0 MPaISO 527
Elongation at Break 220 %Nominal; ISO 527
Elongation at Yield 32 %ISO 527
Tensile Modulus 400 MPaISO 527
50% Modulus 0.0270 GPa
@Strain 50 %
ISO 527
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 125 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK855 / 243063

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.